Forklift Repair Call-out
A container forklift bent, twisted and out of action. One Saturday call, fast response, straight back to work.
Rust is steel turning back into iron oxide. It takes sound metal away and leaves something with no useful strength that takes up more room than the steel it replaced. That second part does most of the damage: expanding rust forces a seam open on a tube, lifts a weld off a plate and cracks the concrete around a post.
A coating is doing a different job. Paint, powder coat and galvanising exist to keep water and salt off the steel. When a coating gives up it blisters, flakes, chalks or stains, and all of that looks alarming while the metal underneath is still sound. The reverse matters more: a rail can carry a tidy coat of paint right up to the morning a post snaps, because the rust was working inside the tube, at the ground line, or behind a fixing where there was nothing to see. So the question is never how bad it looks, it is how much sound metal is left and where it sits in the load path.
Nearly every rust job falls into one of four patterns, and the pattern decides the repair. Skipping this step is how people end up recoating something that needed replacing, or replacing something that needed a wire brush and a tin of primer.
An even orange-brown film on bare or thinly coated steel. It brushes back to clean, bright metal with no depth behind it. Surface rust is a coating problem, not a structural one: clean it back, treat it, recoat properly and the piece carries on.
Holes that go down into the metal rather than across it, concentrated where salt collects and water cannot drain. Pitting is worse than it looks because each pit concentrates stress at its base. We probe pits rather than eye them off, since a pit under a scab of rust is often twice the depth it appears.
Metal that has genuinely gone: a tube wall thinner than it was made, an angle that has lost its edge, a base plate eaten through. Lost thickness cannot be argued back with a bead of weld, so this is the finding that changes the answer. We tap, probe, and where it matters cut a small inspection window in a face carrying no load.
Rust that started at a chip, a cut edge, a weld or a fixing and ran sideways under paint that still looks intact. Press it and the coating gives like a crust over a hollow. This is what gets missed on a walk-past, and why we scrape and sound a rail instead of eyeing it off from two metres away.
Ground out to clean metal, rewelded full depth and then reinforced, because a crack that is simply filled comes back in the same place.
Joints tacked rather than welded, run on one side only, or laid onto rusty steel so the bead never fused, get cut back to sound metal rather than built up over old work.
New steel sized to the weight it actually carries, welded to a face with enough sound metal left to hold it.
Where rust inside a hollow section has forced the seam open, the split length comes out and new tube goes in, because welding a split closed just seals the rust in with the moisture that caused it.
The ground line is where posts die, so the rotted length is cut out and new steel welded in, with the joint clear of where water sits.
Posts grouted into concrete, rails into brickwork, base plates on a slab edge. Where rust in a fixing has cracked the material around it, the fixing is the repair and rewelding the rail above achieves nothing.
Hot-dip galvanising to AS/NZS 4680 is the best protection most structural steel will ever have, and it is also what a repair most often ruins. Heat destroys the coating around a weld and a grinder removes it outright, and welding through galvanising gives off zinc fumes, so the coating gets pulled back with ventilation before the arc is struck.
What happens next separates a repair that lasts from one that rusts out at the weld within a season. Repairing damaged galvanising is a normal, recognised step, and AS/NZS 4680 accepts more than one method: cold galvanising paint, thermal zinc spray and proprietary zinc sticks are all used, and which suits depends on the piece and where it has to live. We cut the coating back, weld, then re-protect the bare metal before leaving, and if a piece is better off going back through a galvaniser we say so. The same thinking shapes new work through our custom metal fabrication and welding and metal fabrication.
The Illawarra is harder on metal than most of the country and it does it in a narrow band. A few streets back, sheltered from the weather, coated mild steel lasts a long time. Within sight of the water, with salt carried in and nothing washing it off, the same steel in the same coating is a different proposition. Two places take it first: the ground line on posts, where salt, soil moisture and poor drainage work the steel from both sides, so a post looks sound at eye height and is hollow at the bottom; and every cut edge, weld and fixing, where the coating is thinnest or absent.
Stainless needs describing honestly, because it often is not. Both 304 and 316 can tea-stain near the coast, and that brown film is cosmetic rather than the metal failing. Grade 316 resists chloride pitting better than 304, which is the real reason to specify it near the water, but it is not stain-proof. Surface finish and regular fresh-water rinsing are what control staining. We will tell you which grade suits your position rather than default to the dearer one, and the same logic drives material choice on new gates, handrails and balustrades across all our Illawarra and South Coast service areas.
Aluminium does not rust, and that true statement gets stretched into a claim that it will not corrode, which is wrong. In salt air aluminium pits: the surface goes dull and chalky, then develops small white-grey craters that work down into the metal the way rust pits go into steel.
The bigger problem is galvanic attack where aluminium meets stainless or steel fixings. Put a stainless screw through an aluminium rail, add salt-laden moisture, and the aluminium around the fixing corrodes away while the screw looks perfect. That is why aluminium rails and gates go loose at the fixings first, and why the fix is to isolate the two metals with nylon washers or sleeves rather than fit a bigger screw into the same hole. Repairs to aluminium and thin-wall stainless are TIG work; mild steel and thicker section are MIG.
Cast iron turns up on older properties in gates, fence panels, brackets, balusters, grates and columns, and it is a different job to welding steel. It is brittle and does not tolerate the shrinkage that follows a hot weld cooling quickly, so the crack after a careless repair sits beside the weld rather than in it.
There are two accepted ways to do it: pre-heat the part, weld it and bring it down slowly so weld and parent metal shrink together, or weld cold with nickel rod in short runs, peening each run and letting the part stay cool between them. Both work, and anyone who says there is only one approach is working from habit. Both take longer than a steel repair, so cast iron quoted as a five-minute weld is a warning sign. We will say whether a cast piece is worth repairing, and will not put a number of years on it afterwards, because that cannot be predicted.
You can weld almost anything once. Whether it stays welded, and whether the piece around it is worth the welding, is the question we answer before quoting. We advise against a repair when section loss is widespread rather than local. One rusted post base in an otherwise sound run is a straightforward cut-out. Six of them, with thin walls between, means the whole run has aged together and fixing one spot just moves the failure along. Same answer when the metal around a joint is too thin to hold a weld that carries load, or when reaching the corrosion means stripping so much of the piece that you have paid for a replacement and got a repair.
Design is the other honest reason to stop. Plenty of metalwork we see did not fail because it rusted. It rusted because it was built in a way that holds water, built light for the span, or built without a brace on a gate wide enough to need one. Repairing that returns you to the same failure on a slower clock, so the useful answer is what a replacement would do differently.
Compliance pushes some jobs the same way. A barrier is required where the fall is 1 metre or more, at a minimum height of 865mm above the nosing line of stairs and above ramps, and 1m above landings, balconies and other floors. No gap may let a 125mm sphere pass, reducing to 40mm where the opening is at the edge of the floor. Where the fall exceeds 4m there must be no horizontal or near-horizontal elements between 150mm and 760mm above the floor that a child could climb. Barrier loads come from AS/NZS 1170.1 and wind from AS 1170.2. Patching a corroded rail that sits well outside those figures leaves you paying for a barrier that still does not comply.
When we say no you get the reasons, in writing if you need them for a landlord or an owners corporation. Being told a piece is finished is worth more than being sold a weld that fails after the invoice clears.
Two photos, one close and one far enough back to show the whole piece and how it is fixed, usually tell us what sort of problem it is. Anything load-bearing gets looked at in person.
We scrape, tap and probe, check the ground line on every post and look behind fixings to work out whether it is surface rust, pitting, section loss or creep. That is where you get told if the answer is replacement.
What gets cut out, what gets welded in, how the bare metal will be protected and what is deliberately left alone, with a price against it, plus anything that will need attention later so it is not a surprise.
Welds dressed back, damaged galvanising repaired or bare steel primed and coated, dissimilar metals isolated at the fixings, and gates and rails adjusted before we leave. Most of it happens at your place as mobile welding, with only pieces needing bench accuracy or a sprayed finish going through the workshop.
Most rust repairs never get near this, but the lines on residential work in NSW are worth knowing. A written contract is required over $5,000 including GST. A small works contract covers $5,000 to $20,000, and more than $20,000 requires a full home building contract, with home building compensation cover and its certificate. The maximum deposit that may be requested is 10 per cent on jobs of any size. Variations should be agreed in writing before the varied work happens, which matters more on corrosion work than anything else, because you do not know what is left until the piece is opened up. We work licensed and insured.
If something metal on your place is rusting, cracked, loose or does not feel right to lean on, send photos through our contact page or call 0413 147 335. You will be told which rust pattern you have, whether it is a weld, a section replacement or a piece that is finished, and what it takes either way.
Plant, trailers and anything on wheels sits under machinery and trailer repairs. A list of smaller jobs around a house or a tenancy, rather than one failed piece, belongs under property maintenance.
Corrosion and cracked-weld repairs on rails, gates and brackets
Real jobs from our own crew, filmed on site. See all our work videos.
A container forklift bent, twisted and out of action. One Saturday call, fast response, straight back to work.
Send a photo and a short description. You get a straight answer on what it needs and what it costs before anything starts.
Rusted metal can be welded, but not while the rust is still there, because a weld will not fuse properly to corroded steel. It has to be ground back to clean, bright metal first. The real question is how much sound metal is left. If the wall thickness is still there, it is a repair. If the steel has lost real thickness around the joint, no amount of weld restores that, and the answer is to cut the section out and weld new steel in, or replace the piece.
Appearance is a poor guide in both directions. A rail can look terrible and be structurally fine if the rust is only on the surface, and it can look freshly painted while a post is hollow at the ground line. Push against it, then look specifically at the base of each post, at every weld, and at every fixing into brick or concrete, because that is where failures start. If a rail moves, if the coating gives like a crust when you press it, or if rust staining is running out of a fixing, have it checked properly rather than judged by eye.
Usually not. If the frame above the damage is sound, the rotted section is cut out, new steel is welded in and the repair is protected again. Replacement becomes the better answer when rust has gone through in several places at once, when the frame has lost real wall thickness generally, or when the gate was built too light or without a brace for the opening it covers. In that last case a repair returns you to the same failure, just later.
Yes, with the coating cut back first and with ventilation, because heating galvanising gives off zinc fumes. The weld destroys the coating locally, so the bare metal has to be re-protected afterwards or it will rust out at the weld. Repairing damaged galvanising is a normal part of the job, and AS/NZS 4680 accepts several methods, including cold galvanising paint, thermal zinc spray and proprietary zinc sticks. Which one suits depends on the piece and where it is going to live.
No. Both 304 and 316 can tea-stain near the coast. Grade 316 resists chloride pitting better than 304, which is the genuine reason to specify it close to the water, but it is not stain-proof and nobody should sell it to you as stain-proof. Surface finish and regular fresh-water rinsing are what actually control staining over the life of a rail.
Aluminium does not rust, but it does corrode. In salt air it pits, going from dull and chalky to small craters that work down into the metal. It also suffers galvanic attack wherever it contacts stainless or steel fixings, which is why aluminium rails usually go loose at the screws first while the screws themselves look perfect. The fix is to isolate the two metals with nylon washers or sleeves, not to fit a larger fixing into the same corroded hole.
Cast iron can be welded. There are two accepted approaches: pre-heat the part, weld it and cool it slowly, or weld cold with nickel rod in short runs, peening each run and letting the part stay cool in between. Both are legitimate and both take longer than a steel repair, because cast iron is brittle and cracks beside the weld if it shrinks too fast. What we will not do is tell you how many years a repaired casting will last, because that cannot be predicted.
Most rust and weld repairs get done where the metal already is. Pulling a gate or a rail off, carting it somewhere and bringing it back adds two trips and a refit to a job that is often a short weld on site. Pieces that need bench accuracy to stay square, or a sprayed finish that cannot be applied in a driveway, get measured on site, built in the workshop and fitted in one visit.
“Finally found someone who actually turned up when he said he would!”
“Cheerful, quick, and didn't try to upsell me on things I didn't need. Rare these days.”
“Turned a weekend-long headache into a one-visit fix. Absolute legend.”